Hi, Does anyone have experience with LOR3A (w/ 1827) on borosilicate glass. The processing parameters, i.e. undercut rate after a 6 min 150C bake, appear quite different than those for silicon. That is, I am seeing a much lower undercut rate for the borosilicate than for silicon. Thank you, Michael _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk