Hi, I am searching for a silane coupling agent for the bonding of glass and polymer (FEP films) . For bonding purposes I have to go up to 260°C, are there coupling agents or adhesives available which can stand this temperature. kind regards, ----------------------------------------------- Fahd Ali _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk