Gary Hillman / S-Cubed
2013-09-18
Hi I agree with Bill however HM DSV preprime at about 200° C might very well
work as well Gary

Sent from my iPhone

On Sep 18, 2013, at 6:07 PM, Fahd Ali  wrote:

> Hi,
> I am searching for a silane coupling agent for the bonding of glass and
polymer (FEP films) . For bonding purposes I have to go up to 260°C, are there
coupling agents or adhesives available which can stand this temperature.
>
> kind regards,
> -----------------------------------------------
> Fahd Ali
>
>
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply