I agree with Bill however HMDS could very well work in a vapor prime Gary Sent from my iPhone On Sep 19, 2013, at 1:32 AM, Bill Moffatwrote: > Hi,there are numerous silanes that can act as a bonding agent for Polymers to glass. The most common one is Amino Propyl Tri Ethoxy Silane, APTES. It has a different vapor pressure to HMDS the most common bonding silane for photoresist. A common process is APTES vapor, Polymer coating then bake up to 450 degrees C with no problems. Bill Moffat > > -----Original Message----- > From: mems-talk-bounces+bmoffat=yieldengineering.com@memsnet.org [mailto:mems- talk-bounces+bmoffat=yieldengineering.com@memsnet.org] On Behalf Of Fahd Ali > Sent: Wednesday, September 18, 2013 2:08 AM > To: mems-talk@memsnet.org > Subject: [mems-talk] adhesion agents > > Hi, > I am searching for a silane coupling agent for the bonding of glass and polymer (FEP films) . For bonding purposes I have to go up to 260°C, are there coupling agents or adhesives available which can stand this temperature. > > kind regards, > ----------------------------------------------- > Fahd Ali > > > _______________________________________________ > Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. > Visit us at http://www.mems-exchange.org > > Want to advertise to this community? See http://www.memsnet.org > > To unsubscribe: > http://mail.mems-exchange.org/mailman/listinfo/mems-talk > _______________________________________________ > Hosted by the MEMS and Nanotechnology Exchange, the country's leading > provider of MEMS and Nanotechnology design and fabrication services. > Visit us at http://www.mems-exchange.org > > Want to advertise to this community? See http://www.memsnet.org > > To unsubscribe: > http://mail.mems-exchange.org/mailman/listinfo/mems-talk _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk