Hi,

I was wondering if anyone can suggest me thick permanent photoresist (70-100um)
single spin. I know of SU-8 but I need resists which have lower CTE~ (as low as
20ppm/C) or close.

Many Thanks,

Ricky Anthony
Tyndall National Institute