Hi,

Thanks for your reply. I have looked into KMPR. But I am not sure of its CTE. I
asked the company, but was told that since it is developed for molding purposes,
CTE of KMPR was ignored.

So, I was wondering if there is thick resist, with low CTE. Or any Polyimides
which can give me a thickness of (70-100um, highly unlikely).

Many Thanks,
Ricky


-----Original Message-----
From: mems-talk-bounces+ricky.anthony=tyndall.ie@memsnet.org [mailto:mems-talk-
bounces+ricky.anthony=tyndall.ie@memsnet.org] On Behalf Of TOPART Patrice
Sent: 23 September 2013 18:42
To: 'General MEMS discussion'
Subject: Re: [mems-talk] Thick Permanent Photoresist

Have you looked at KMPR?



Patrice Topart, PhD
Gestionnaire de groupe, Microfabrication Group Manager Microfabrication INO
2740 Einstein
Québec, Qc, Canada
G1P 4S4
G Tél/Phone: 418-657-7406, 2502
/  Fax: 418-657-7009
  Email: patrice.topart@ino.ca
: WWW: www.ino.ca

-----Message d'origine-----
De : mems-talk-bounces+patrice.topart=ino.ca@memsnet.org [mailto:mems-talk-
bounces+patrice.topart=ino.ca@memsnet.org] De la part de Ricky Anthony Envoyé :
Monday, September 23, 2013 5:02 AM À : mems-talk@memsnet.org Objet : [mems-talk]
Thick Permanent Photoresist

Hi,

I was wondering if anyone can suggest me thick permanent photoresist (70-100um)
single spin. I know of SU-8 but I need resists which have lower CTE~ (as low as
20ppm/C) or close.

Many Thanks,

Ricky Anthony
Tyndall National Institute
Ireland
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider
of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

********************************************************************************
**
Ce courrier  lectronique s'adresse uniquement   la personne d sign e ci-dessus,
il est confidentiel et ne doit pas  tre remis   une autre personne, ni reproduit
et son contenu ne peut  tre autrement divulgu .
Si ce courrier  lectronique vous est transmis par erreur, veuillez nous en
avertir imm diatement   l'adresse securite@ino.ca. Nous vous remercions de votre
collaboration.

This email is directed in confidence solely to the person named above, and may
not otherwise be distributed, copied or disclosed. If you have received this
email by error, please notify us immediately by email to address
security@ino.ca. Thank you for your cooperation.
********************************************************************************
**
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply