Hello, Girija Moona, I saw your recent cantilever question on mems-talk and I'd be happy to give you all the information we have on fabrication procedures. I'm relatively new to MEMS/nanotech research but I've been doing it (with undergraduate research students) for several years and we have successfully constructed micro-bridges and cantilevers. I'll send a write-up of our work to your email address. Feel free to ask me any questions you might have, in particular, requests for more detailed instructions, since that is the sort of information that is often hard to glean from research articles (I know!). Regards, Jeff Wolinski Prof. Jeffrey P. Wolinski Department of Physics Grove City College, Faculty Box 3137 100 Campus Drive Grove City, PA 16127-2104 Voice: 724-458-2201 Fax: 724-458-2181 There is no expedient to which a person will not resort to avoid the real labor of thinking. - Sir Joshua Reynolds A democracy cannot exist as a permanent form of government. It can only exist until the voters discover that they can vote themselves largesse from the public treasury. From that moment on, the majority always votes for the candidates promising the most benefits from the public treasury with the result that a democracy always collapses over loose fiscal policy, always followed by a dictatorship. The average age of the world's greatest civilizations has been about 200 years. These nations have progressed through this sequence: From bondage to spiritual faith; From spiritual faith to great courage; From courage to liberty; From liberty to abundance; From abundance to selfishness; From selfishness to apathy; From apathy to dependence; From dependence back into bondage. - source unknown _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk