Hi I have a few questions about hexamethyldisilazane or HMDS (CH3-Si-NH2-Si-CH3) 1. 1. Is HMDS a polar molecule? Is there any dipole present? electronegativity values of constituents are : H 2.2, C 2.55, Si 1.9, N 3.04. Carbon (2.55) - flourine (4) bonds are polar because of their electronegativity difference. 2. 2. How thick can HMDS on top of SiO2-Si be when it is dried in air from a liquid state? Can the thickness of HMDS be determined when it is air dried? 3. If HMDS is air dried and some molecules are left in sample, is it going to be HMDS molecule or it will be something else? Will it release ammonia? Also will it be a continuous layer or there will be clustering? Thanks a lot :) regards Sk _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk