Hi Debashis,

look at Loctite Medical Device Adehesives:

http://www.henkelna.com/industrial/medical-device-adhesives-17800.htm



Regards
André

-----Ursprüngliche Nachricht-----
Von: mems-talk-bounces+aboedecker=imsas.uni-bremen.de@memsnet.org
[mailto:mems-talk-bounces+aboedecker=imsas.uni-bremen.de@memsnet.org] Im
Auftrag von DEBASHIS MAJI
Gesendet: Montag, 6. Januar 2014 07:28
An: General MEMS discussion
Betreff: [mems-talk] Bio-compatible epoxy

Dear All,

I am searching for a some biocompatible epoxy (not conductive epoxy) to fix
my sensor over a substrate for some in vitro animal experiments. can anybody
kindly provide me names of few such epoxies?

Thanks in advance.

--
Thanks & Regards

Debashis Maji,
Senior Research Fellow,
PhD Scholar - School of Medical Science & Technology, IIT Kharagpur, India -
721302 _______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply