Do you mean like T-shirt production? If so, seems like when you lift the screen off the substrate you'd get streaking. On Mon, Jan 27, 2014 at 2:53 AM, Janis Klavinswrote: > Hello, > > I am trying to coat a SU-8 using screen printer. Has anyone tried this > method instead of using spin coater? And do you have any tips or tricks for > this method? > > -- > Best regards, > Mr. Janis Klavins > EuroLCDs > Phone: +37163600300 > Mobile: +37126141049 > > _______________________________________________ > Hosted by the MEMS and Nanotechnology Exchange, the country's leading > provider of MEMS and Nanotechnology design and fabrication services. > Visit us at http://www.mems-exchange.org > > Want to advertise to this community? See http://www.memsnet.org > > To unsubscribe: > http://mail.mems-exchange.org/mailman/listinfo/mems-talk -- -Nathan _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk