In the past I have made use of the maskmaking facilities of a South African
company called PICO Systems, and I can strongly recommend them for this service.
For research purposes their work quality certainly matches that of the better
known vendors. They have a web site at  http://www.pico.co.za  and Bruno Meyer
is the contact person for photomask manufacturing; he can be reached at e-mail:
bmeyer@csir.co.za.

James van de Vyver
----------
>
> Could people give me recommendations for a vendor who will produce patterned
> 5" chrome photomasks for universities at a decent price to be used in a
> 1:1 contact aligner. I have several masks to be made.
>
> Thanks,
> Kevin Walsh
>
> --
> Dr. Kevin M. Walsh
> Electrical Engineering Department, Speed Scientific School
> University of Louisville, Louisville, KY 40292
> (502) 852-0826
>
> Internet address: kmwals01@starbase.spd.louisville.edu
>
>


reply