Dear MEMS Researchers,

Would any of you know the thermal conductivity (k) of the MUMPS Poly 1 layer?

According to the Ted Kamins book, "k" should lie between 30 and 120 W/mK,
depending on the grain size of poly. But I need a more accurate number.

Thanks,
Shivalik