> Hello,
> I'm looking for a method to produce circular membranes etched
> from Si. The membrane itself can be made of any material eg
> Si3N4 or SiO2 or Si itself. Can anyone help?
>
> Thanking you in advance
>
> Phil Rayner
>
>

Microfabrication using DRIE (deep reactive ion etching) can produce these.
MCNC provides DRIE for a fee.


--