John, Many prepress bureaus output to film at 5080 dpi now which is a raster size of 5 microns. We regularly have our masks made at this resolution and have been very satisfied. Check your Yellow Pages under desktop publishing. -Mark. > I have recently used a commercial printer to make a mask on printer's >film. He used a Linotronic printer with 2540 dpi. The mask gave us about 25 >micron resolution, which I understand is pretty typical. > I would really like about 10 micron resolution, but our >photolithography system does not have reduction capability (only 1:1). Does >anyone know how to get closer to 10 microns? Try to find higher dpi >capabilities? Commercially available reduction to make a new mask from the >existing mask? > Any suggestions would be appreciated. > >John Lodmell >John.Lodmell@aero.org > -------------------------------------------- Mark Bachman, Ph.D. mbachman@uci.edu / 949-824-6421 (-3732 fax) Research Physicist, Microsystems Engineering University of California at Irvine