> Hi, > > I'm looking for resists that can be spun up to around 25 microns and have > good compatability with alkaline (pH=10) gold sulfite plating bath. We are > using SJR 3740 but are interested in other alternatives. We tried SU-8 > but can't find anything to remove it. Is there anything else available? > > Thanks, > > Todd Green > > I have been using shipley 5740 with thickness up to 52um for this type of application. -- Keith Jackson Lawrence Berkeley National Laboratory Berkeley,Ca 94720 510-486-6894 voice 510-486-4955 fax