Hello,

In regard to your question about etching microchannels on glass, there is an
excellent article in the Journal of Biomedical Microdevices 1:1, 7-26, 1998
"Microfabrication Technology for the Production of Capillary Array
Electrophoresis Chips" Peter C. Simpson, Adam T. Wooley, and Richard A.
Mathies.  This research group is at Berkeley, Dept of Chemistry,
rich@zinc.cchem.berkeley.edu

John West
Microcosm Technologies
CAD for Microfluidics
www.memcad.com