MUMPs7 Announcement
Reminder!
The 7th ARPA-supported Multi-User MEMS Processes (MUMPs) run design deadline is
scheduled for February 27, 1995.
MUMPs is available to all domestic (USA and Canada) industry, academic and
government parties. Participants may purchase a 1 cm x 1 cm die location for
$500 with approximately 15 unreleased die delivered. Layout service and die
releasing are available at an additional cost.
Design rules and process specifications are available from MCNC. Please send
email to cash@mcnc.org asking for the MUMPs design rules. Please include your
snailmail address, phone and fax numbers.
***Please note, if you already have a design rule document, be sure it is
revision 3 (10/94).***
For more information or to reserve a die location, send email to Dave Koester "
koester@mcnc.org" or call 919-248-1493.
The following is the tentative schedule for future runs.
Run Name Design Deadline
MUMPs8 5-15-95
MUMPs9 8-14-95
MUMPs10 11-13-95
MUMPs11 1-15-96
MUMPs12 3-11-96
MUMPs13 5-13-96
MUMPs14 7-15-96
MUMPs15 9-16-96
MUMPs16 11-11-96