Robert: I believe we met at MEMS 99. BSAC did a project plasma etching Teflon, very nice work. Their review meeting is next week. There are some sodium based etches which serve as adhesion promoters before adhesives are applied. Jon Bernstein At 05:34 PM 3/8/99 -0700, you wrote: >Folks, > >I am compiling information on Teflon, but the etching characteristics have been >particularly elusive. > >Can anyone help in this regard? Information on its molding will also be >appreciated. > >Thank you. > >Robert. > >-- >Robert S. Okojie, Ph.D. >Senior Engineer >Ford Microelectronics >9965 Federal Drive, Colorado Springs, CO 80921-3698 >Phone:(719)528-7727; Fax: (719)528-7529 >"The frontier of knowledge has no boundary. Paradigms rise and fall" > > Jonathan Bernstein MEMS Technology Center Draper Labs, MS 37 555 Technology Square Cambridge, MA 02139 USA jbernstein@draper.com Tel. (617) 258-2513 Fax (617) 258-4238