durusmail: mems-talk: Re: How does everybody cut the glass? (7740)
Re: How does everybody cut the glass? (7740)
Re: How does everybody cut the glass? (7740)
Wen H. Ko
1999-03-23
Cut it with diamond saw as with Si or scrape lines with diamond tips then
break.
wen ko

At 11:05 AM 3/17/99 +0800, you wrote:
>Hi, everybody:
>    I am micromachining on 7740 glass, but I have problem to cut my 7740
>glass into pieces, in order not to waste when experiments...
>    Does anybody have good comments for me? or some experience to share...
>thanks!
>Best regards,
>____________________________________________
>Jerry Lee
>(Jia-Hong Lee)
>Insitute of Applied Mechanics,
>National Taiwan University
>Taipei, Taiwan, ROC
>e-mail:
>iamjhlee@email.com
>r6543023@gauss.iam.ntu.edu.tw
>"Try then error is better than no try"
>
>
>
>
Wen H. Ko
Phone: 1-216-368-2071
FAX: 1-216-368-5326
e mail: whk@po.cwru.edu