Hi, Wen H. Ko: But thin glass as 500mu m is very fragile, can it be well cut with diamond saw? ____________________________________________ Jerry Lee (Jia-Hong Lee) Insitute of Applied Mechanics, National Taiwan University Taipei, Taiwan, ROC e-mail: iamjhlee@email.com r6543023@gauss.iam.ntu.edu.tw "Try then error is better than no try" >Cut it with diamond saw as with Si or scrape lines with diamond tips then >break. >wen ko > >At 11:05 AM 3/17/99 +0800, you wrote: >>Hi, everybody: >> I am micromachining on 7740 glass, but I have problem to cut my 7740 >>glass into pieces, in order not to waste when experiments... >> Does anybody have good comments for me? or some experience to share... >>thanks! >>Best regards, >>____________________________________________ >>Jerry Lee >>(Jia-Hong Lee) >>Insitute of Applied Mechanics, >>National Taiwan University >>Taipei, Taiwan, ROC >>e-mail: >>iamjhlee@email.com >>r6543023@gauss.iam.ntu.edu.tw >>"Try then error is better than no try" >> >> >> >> >Wen H. Ko >Phone: 1-216-368-2071 >FAX: 1-216-368-5326 >e mail: whk@po.cwru.edu