The following company will provide Si-on-glass LPCVD process. However, you
need to send them your CLEAN glass wafers.
STRATAGLASS Thin Film Services
958 San Leandro Ave., #100
MOUNTAIN VIEW, CALIFORNIA 94043
650-988-1700
FAX:650-988-1739
email: strataglas@earthlink.net
www.strataglas.com
Good luck.
Shenheng Guan
Symyx Technologies
3100 Central Expressway
Santa Clara, CA 95051
408-764-2035
408-748-0175(FAX)
sguan@symyx.com
-----Original Message-----
From: Lee Jia-Hong [mailto:r6543023@iam.ntu.edu.tw]
Sent: Sunday, April 11, 1999 1:50 AM
To: MEMS@ISI.EDU
Subject: Polysilicon on glass source?
Hi, everybody:
Can anybody tell me where to buy polysilicon-on glass? this glass must
be capable of bonding to silicon...
I really need...
Thanks!
Best regards,
____________________________________________
Jerry Lee
(Jia-Hong Lee)
Insitute of Applied Mechanics,
National Taiwan University
Taipei, Taiwan, ROC
e-mail:
iamjhlee@email.com
r6543023@gauss.iam.ntu.edu.tw
"Try then error is better than no try"