For a quick response, here are some numbers that would get you going.. Density = 2330 Kg/m^3 Specific heat = 753 J/Kg C Thermal conductivity = 125 W/m K CTE = 9.4 x 10^-6 /C heat capacity = density*specifc heat For detailed information, you can look up the mems property data base at isi.edu Regards, Ram -=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-= Ram N. Ramanan, Ph.D., PE, Member of Technical Staff FSI International, MS 5-7060, 600 Millennium Dr., Allen, TX-75013 Email: nramanan@fsi-intl.com, ?FSI: http://www.fsi-intl.com Phone: 972-643-2213, Fax: 972-643-2292 -=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-= "Liu Yanju (Dr)" To: MEMS@ISI.EDUSubject: Thermophysical properties of polysilicon 03/29/2000 19:05 Please respond to "Liu Yanju (Dr)"; Please respond to mems-cc To MEMS colleagues: Can anyone provide me with information about thermophysical properties of polysilicon such as thermal conductivity, specific heat and heat capicity Thank you very much. Liu Yanju, Ph. D Micro Machine Lab School of MPE Nanyang Technological University Singapore