Mr. Crawford,

SU-8 can be purchased from MicroChem Corp. (MCC). They sell in
500 mL, 1 L, and 4 L bottles. The contact information is:

   MicroChem Corp.
   1254 Chestnut Street
   Newton, MA 02464-1418
   phone: (617) 965-5511
   fax: (617) 965-5818
   web: www.microchem.com

EV Group has conducted extensive SU-8 testing with great success.
If you would like SU-8 application notes, or to discuss this,
please email info@evgroup.com (mailto:info@evgroup.com).

Best Regards,

Josh Palensky
EV Group Inc
Tel: (602) 437-9492
Fax: (602) 437-9435
Email: j.palensky@evgroup.com
Web: www.EVGroup.com


-----Original Message-----
From: Gregory Crawford [mailto:Gregory_Crawford@brown.edu]
Sent: Friday, July 21, 2000 8:35 AM
To: MEMS@ISI.EDU
Subject: Where do I buy SU-8


Can someone tell me where I can by the SU8 epoxy ?

You help is much appreciated,

Greg Crawford
Brown University
Gregory P. Crawford
Brown University
Division of Engineering, Box D
182 Hope Street
Providence, Rhode Island  02912
401-863-2858 (voice)
401-863-9120 (fax)
Gregory_Crawford@Brown.Edu