Greg,

EVGroup has worked with MCC, the manufactures of SU-8, to generate spin
curves and starting process parameters.  Please see the MicroChem Corp
contact information below.  If you would like a bound copy of our SU-8
applications notes please contact us at info@evgroup.com 
.

Rob Hardman or Scott Heideman
Technical Sales Representative
Tel: (617) 965-5511
Fax: (617) 965-5818
E-mail:  >
MCC Web: >


Best Regards,

Loren St. Clair

EV Group-Technology, Tel: (602) 437 9492 x 109, Fax: (602) 437 9435
E-mail: l.stclair@evgroup.com  , Web:
www.EVGroup.com  , Date: 8/4/2000



                -----Original Message-----
                From:   Gregory Crawford [mailto:Gregory_Crawford@brown.edu]
                Sent:   Friday, July 21, 2000 8:35 AM
                To:     MEMS@ISI.EDU
                Subject:        Where do I buy SU-8

                Can someone tell me where I can by the SU8 epoxy ?

                You help is much appreciated,

                Greg Crawford
                Brown University
                Gregory P. Crawford
                Brown University
                Division of Engineering, Box D
                182 Hope Street
                Providence, Rhode Island  02912
                401-863-2858 (voice)
                401-863-9120 (fax)
                Gregory_Crawford@Brown.Edu


reply