Dear Glenn,

We are working on a process for applying a electroless mixture onto an
activated surface at room temperature to metallize the substrate.  We have
used painting and other means of application including silk screening would
be practical.  The process is electroless and works for copper and silver
and we have done a few tests with gold.  The substrate would have to be
sensitized as in conventional electroless.  We also provide nanosize metal
powders that can be incorporated into such mixtures.  If you have any other
questions just drop me an e-mail.


Cheers,

Cindi Prorok
Argonide Nanomaterials
www.argonide.com


Glen Smith wrote:

> Hi there,
>
> Looking for vendors that will do gold electroless
> plating for 6" wafers.  Or any vendor that will
> sell the equipment or supplies for it?
>
> Thanks
>
> glen
> ________________________________________________________________________
> Get Your Private, Free E-mail from MSN Hotmail at http://www.hotmail.com
>
>


reply