Hello, You can ask ALCATEL Vacuum Technology http://www.alcatel.com/cable/hvt/ They have special expertise in leak testing and in semiconductor market. Best regards. gene_gan@am.exch.agilent.com wrote: > Hi, there, > > I am looking for a method to test the leakaging rate of the hermetic > sealed micro-sensors. The device has a dimension of 1mm x .8mm x 0.5mm with > cavity about 0.1 mm^3. My questions are: > 1. Is it possible to use He test to check the leakage rate and how to do > it? > 2. Are there any companies to provide this kind of service? > > Your suggestion is higly appreciated! > > Duke > -- Olivier de Gabrielli - Responsable secteur Mécatronique thésame Immeuble "Le Salève" C. U. F. R. A. F - 74166 ARCHAMPS - France Tel: 33 (0)450 31 55 10 Fax: 33 (0)450 31 57 21 mailto:odegabrielli@c4i.fr http://www.thesame-innovation.com/ _________________________________________________________