In the presence of chrome/gold, discoloration of the polysilicon layers is seen when releasing the MUMPS devices in 49% HF. Anyone out there with an explaination and a possible solution? Thanks Glen ______________________________________________________ Get Your Private, Free Email at http://www.hotmail.com