Sorry this didn't make it through earlier ... let's try again.
-----
Below is a list of all vendors that were recommended by people from
mems@isi.edu, sci.engr.micromachining , sci.engr.manufacturing , and
sci.engr.semiconductors . Many thanks to all who responded.
If a contact is listed, and I do not state otherwise, then I have called to
verify the contact. I have no more information for each of these companies.
I hope you find the list to be useful.
-Steven
-----
Laser Services, Inc.
- laser
- contact Barry Beachesne or Rick Titus
http://www.optoelectronics-world.com/lfw/lfwco/lsrserv.html
123 Oak Hill Rd.
Westford, MA 01886-1198
978-692-6180
Lasair
- laser (YAg for thick silicon)
- Contact Rene Brown or John Richmond
Oceanside, CA.
760-724-6576
760-724-0803
Team Industries
- laser
- contact not confirmed
Priemyselna 1
POBox 208
91700 Trnava
Slovakia
Tel: +421-805-551-3521
Fax: +421-805-551-3521
Pi Medical, Inc.
- UV excimer laser (high precision, low speed)
- contact Jerry Boogaard
16125 SW 72ND AVE
Portland OR 97224
phone 503-639-3100
FX: 503 639-0330
Resonetics
- laser
- CO2 laser for thick items
- contact Dave Wall
http://www.resonetics.com/
4 Bud Way Building 21,
Nashua, NH 03063 USA
Phone: 603-886-6772
Fax: 603-886-3655
Questech
- laser
- contact Dustin Hickman or Randy House
http://www.questlaser.com/
2201 Executive Dr.
Garland, TX 75041
(972).278.8006
(972).278.8036
Applied Laser Technology, Inc.
- laser
- contact Stephen Knight
http://www.altinc.com/
14155 S.W. Brigadoon Ct. Suite B.
Beaverton, OR 97005
PHONE 503-641-4400
FAX 503-641-6696
Clark-MXR
- laser
- contact Bob Maynerd at extension 225
http://www.cmxr.com/
7300 West Huron River Drive
Dexter, Michigan 48130 USA
734-426-2803
Fax: 734-426-6288
Accu-Tech Laser Processing, Inc.
- laser
- contact Jenny Denaco or Sandy Oh
http://www.accutechlaser.com/
1175 Linda Vista Dr.
San Marcos, CA 92069
Phone (760) 744-6692
Fax (760) 744-4963
General Scanning Inc: Lumonics
- laser
- contact John DeGiorgio
http://www.gsilumonics.com/
(one of several locations)
60 Fordham Road, Building 2
Wilmington, MA, 01887
Tel: 1 (978) 661-4300
Fax: 1 (978) 988 8798
Iowa Laser Technology, Inc.
- laser
- contact Sean Abbas
http://www.iowalaser.com/
6122 Nordic Dr.
Cedar Falls, IA 50613
Tel 319-266-3561
Toll Free: (800) 397-3561
Fax: 319-266-8203
North Eastern Materials
- laser
New Hampshire 603-429-2879
South Bay Technology Inc
- wire saw
- machines vendor, but wil do demo cuts
- contact Mike Mizell
http://soutbaytech.com/
1120 Viaduct Callejon
San Clemente, CA 92673
(949) 492-2600
(800) 728-2233
Permacel (Nitto Denko Inc)
- reversable adhesive dicing tape
- product name: revalpha
encapsulated beads which burst and kill the adhesion, should not
cause contamination of underlying or nearby surface
- contact Richard Mumber at 732-418-2546 for tech info
http://www.permacel.com/
(sales) 1-800-755-8273
Synova
- water jet/laser
- contact not confirmed
http://www.synova.ch
Parc scientifique/EPFL
1015 Lausanne
Switzerland
TEL ++41 (0)21 693 8371
FAX ++41 (0)21 693 8370
Prejet Precision Techniques Ltd.
- (using Synova's waterjet)
- contact not confirmed
http://www.prejet.com/
Huenibachstrasse 58
CH - 3626 Huenibach
Tel ++41 33 243 06 60
Fax ++41 33 243 06 61
Integrated Reliability Corporation
- focused ion beam (cut depth: several microns)
- contact Don Lyons
http://www.irsi.com/
10225 Barnes Canyon Road
San Diego, California 92121 USA
Telephone: (619) 658-9770
FAX: (619) 550-9445
info@irsi.com
Accurel
- focused ion beam (cut depth: several microns)
- contact Sandra Delgotto
http://www.accurel.com/
785 Lucerne Drive
Sunnyvale, CA 94086
General: 408/737-3892
Fax: 408/737-3916
Sales: 408/737-3892
Sales Email: arams@accurel.com
Ion Beam Milling, Inc
- ion beam (cut depth: several microns)
- contact Debby Marcotte
1000 E Industrial Park Dr
Manchester, NH 03109
(603) 644-2326
----------------- Original message follows -----------------
At 09:58 AM 11/10/99 , you wrote:
>Hello to everyone,
>I searched through the archives of these groups but did not find references
>to specific services, so here is my question.
>
>Could you please send the names and numbers of any laser cutting services
>known to you, any area of the country is fine. I'd like to use this method
>to separate some die which contain very fragile mechanical devices and are
>also very sensitive to moisture. I am assuming that laser methods (optical
>or "CO2 lasers") are fairly gentle. A typical die saw could ruin my devices.
>
>Also, if you know of gentle die-sep methods other than the above, please
>send information.
>
>Thank you,
>-Steven
>
>