Hi,

Does anyone know of an etchant that will attack my oxide sacrificial layer but
not the nitride or aluminum. I have tried straight HF and it seems to work
quite alright but I am looking for a better solution. It has to be a wet
etchant. Thanks in advance.

Regards
Yan