Times Patrick T. Moseley Manager, Electrochemistry, International Lead Zinc Research Organization Inc. P. O. Box 12036, Research Triangle Park, N. C. 27709 Tel. (919) 361 4647 Fax. (919) 361 1957 MonacoDear collegues, Which company or institute can help me with sputtering gold and platinum. I have some substrates approx. 1 inch by 1 inch that I need to coat. Initially I need to experiment with thickness of the deposit. I do not want to invest in a sputter unit and targets just yet, but would be willing to pay for this first "look-see" work. Thanks Patrick T. Moseley