durusmail: mems-talk: Re: Looking for Glass Plate(4 inches) Vender.
Re: Looking for Glass Plate(4 inches) Vender.
2001-02-10
Re: Looking for Glass Plate(4 inches) Vender.
Jack Merrin
2001-02-10
Try www.nanofilm.com.  They have very nice chrome 4" glass plates for
about $10.  You may have to etch off the chrome and dissolve the
photoresist.  They also have blanks plates if you ask.

jack


reply