durusmail: mems-talk: Wear rate of Ni(80)-Fe(20) Permalloy
Wear rate of Ni(80)-Fe(20) Permalloy
2001-10-02
Wear rate of Ni(80)-Fe(20) Permalloy
Sanghoon Lee
2001-10-02
Hi,

I'm looking for some experimental data of Ni-Fe permalloy
which has been used as a rotor and bearing material
in a magnetic micromotor (variable-reluctance motor).
Doing the frictional study of that kind of actuators, I need
the wear rate and friction coefficient of the above material.

Could someone provide some data?

Sanghoon Lee
====================================================
Research Assistant
University of Texas - Austin
Dept. of Mechanical Engr.
(512) 471-0968
onandon@mail.utexas.edu
====================================================