Hi,

Does anyone know of a wet etch that attacks Nickel but doesn't touch
aluminum? I would appreciate if you could let us know.

Thanks and regards,
Manish

************************************
Manish Kothari, Ph.D.
Iridigm Display Corporation
2415 Third Street, Suite 235
San Francisco, CA 94107
Ph:   (415) 626-8800, x106
Fax:  (415) 626-9775
email:mkothari@iridigm.com
*************************************


##################################################
This email communication may contain CONFIDENTIAL INFORMATION of IRIDIGM
DISPLAY CORPORATION and is intended only for the use of the intended
recipients identified above. If you are not the intended recipient of this
communication, you must not use, disclose, distribute, copy or print this
email. If you have received this communication in error, please immediately
notify the sender by reply email, delete the communication and destroy all
copies.
##################################################

reply