Alex Shenderov
2001-12-06
There's Foturan available from Microglas http://www.mikroglas.de/ and there
was also a photosensitive glass made by Corning that we tried to get a while
ago but could not.  Good luck.

Alex

-----Original Message-----
From: mems-talk-admin@memsnet.org [mailto:mems-talk-admin@memsnet.org]On
Behalf Of Xiaoyan (Sheri) Wang
Sent: Thursday, December 06, 2001 10:31 AM
To: mems-talk@memsnet.org
Subject: [mems-talk] photosensitive glass


Hi, All,

I'm looking for a type of glass that is photo-etchable or
negative photosensitive. Does anyone know where I can get
it? Any information is greatly appreciated.

Regards,

Sheri
_______________________________________________
mems-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply