Hello Xiaoyan (Sheri) Wang,

Try visiting the MicroGlass web site : http://www.mikroglas.com/index_e.html .
Under "Products" look for the "FOTURAN" photosensitive glass.
You may find this glass useful .

Good Luck,

Danny .
-----------------------------------------------------

Danny Klein
Faculty of Mechanical Engineering
Technion, Israel Institute of Technology
Haifa, 32000
Israel

Tel: 972-4-8292946
Email: dannykl@tx.technion.ac.il

----------------------------------------------------


  ----- Original Message -----
  From: Xiaoyan (Sheri) Wang
  To: mems-talk@memsnet.org
  Sent: Thursday, December 06, 2001 8:30 PM
  Subject: [mems-talk] photosensitive glass


  Hi, All,

  I'm looking for a type of glass that is photo-etchable or
  negative photosensitive. Does anyone know where I can get
  it? Any information is greatly appreciated.

  Regards,

  Sheri
  _______________________________________________
  mems-talk@memsnet.org mailing list: to unsubscribe or change your list
  options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
  Hosted by the MEMS Exchange, providers of MEMS processing services.
  Visit us at http://www.mems-exchange.org/

reply