Hi Sheri

There is a photosensitive glass called Foturan made in Germany - not sure if
it is commercially available yet but here is the web site:
http://www.mikroglas.com

Good luck

Mark Leonard
Manager MISEC cleanroom
Dept. Computing & Electrical Engineering
Heriot Watt University
Riccarton
Edinburgh EH14 4AS

----- Original Message -----
From: "Xiaoyan (Sheri) Wang" 
To: 
Sent: Thursday, December 06, 2001 6:30 PM
Subject: [mems-talk] photosensitive glass


> Hi, All,
>
> I'm looking for a type of glass that is photo-etchable or
> negative photosensitive. Does anyone know where I can get
> it? Any information is greatly appreciated.
>
> Regards,
>
> Sheri
> _______________________________________________
> mems-talk@memsnet.org mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply