durusmail: mems-talk: DRIE STS vs ALCATEL
DRIE STS vs ALCATEL
DRIE STS vs ALCATEL
Sun Yu
2001-12-07
In our ICP, we are not allowed to use metal masks. I heard that once a guy
used a metal mask, it cost a LOT to get the piece of equipment fixed.

Sun

At 04:18 PM 12/7/01 +0100, you wrote:
>Hello,
>
>I know that with Alcatel DRIE engines we can use Al as mask can we do it
>with STS multiplex ICP too ?
>
>Thanks for yoour help
>
>Matthieu
>_______________________________________________
>mems-talk@memsnet.org mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.mems-exchange.org/