FERRO corp sells photoresist that is impregnated with glass.
One would photo-image the substrate,/ burn off the photoresist binder / fire
the glass.

> From: "Xiaoyan (Sheri) Wang" 
> Reply-To: mems-talk@memsnet.org
> Date: Thu, 06 Dec 2001 13:30:40 -0500
> To: mems-talk@memsnet.org
> Subject: [mems-talk] photosensitive glass
>
> Hi, All,
>
> I'm looking for a type of glass that is photo-etchable or
> negative photosensitive. Does anyone know where I can get
> it? Any information is greatly appreciated.
>
> Regards,
>
> Sheri
> _______________________________________________
> mems-talk@memsnet.org mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply