durusmail: mems-talk: lift-off
lift-off
lift-off
Vladimir Gelfandbein
2001-12-10
Hi
You probably need a thin layer of Cr ( even stainless steel) between Pd and
Glass.

Vladimir
Nayna Networks

-----Original Message-----
From: mems-talk-admin@memsnet.org [mailto:mems-talk-admin@memsnet.org]On
Behalf Of Rajsekhar Popuri
Sent: Friday, December 07, 2001 7:09 AM
To: mems-talk@memsnet.org
Subject: [mems-talk] lift-off


Hello,

I am trying to do a lift-off.I sputter coated gold-palladium of 2000A
thickness on a glass wafer.When i tried to do a lift-off with
acetone-methanol,gold-palladium layer was completely peeled off the glass
wafer.Can anyone tell me the reason for this and suggest a suitable process
to do a lift-off with gold-palladium.

Thanks in advance
Rajsekhar.




_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp
_______________________________________________
mems-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply