How thick a coating is necessary?
Any method of growing (even a native oxide) on silicon will cause the
surface to become hydrophillic.  H2O2 exposure will do.

> From: jung hoon yeom 
> Reply-To: mems-talk@memsnet.org
> Date: Tue, 11 Dec 2001 15:11:59 -0600 (CST)
> To: 
> Subject: [mems-talk] any hydrophillic layer?
>
> Dear folks in the mems community
>
> I'd like to do conformal deposition on the Si substrate and modify it to
> hydrophillic surface(not hydrophobic) regardless of its thickness. And I
> am open to any kind of pocessing.
>
> Thanks
>
> Junghoon Yeom   University of Illinois at Urbana-Champaign
> Research Assistant  Department of Mechanical & Industrial Engr
> _______________________________________________
> mems-talk@memsnet.org mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply