Haigh, Richard Daniel
2001-12-13
Hi

PZT can be etched in ~5% etchant solution to water. the etchant solution
being 3:1 HCl:HF by composition. Before etching this solution (of 5% etchant
and 95% water) can be further diluted to about 25% strength with water.

It should be noted that some groups have used an etchant solution based on
HCl, HF and HNO3 - perhaps this will work better for your needs?


Regards


Richard Haigh

-----Original Message-----
From: KunLungYen@itri.org.tw [mailto:KunLungYen@itri.org.tw]
Sent: 12 December 2001 01:40
To: mems-talk@memsnet.org
Subject: [mems-talk] looking for PZT etchant


hi,

does anyone know the etchant for PZT?
thanks in advance.

Kun-lung Yen
_______________________________________________
mems-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply