Luiz Marangoni
2001-12-19
Hi Lior,

Didn4t you consider to grow your thick Al film by electroplating? I think
it could be the solution for your case if your process enable it.

Best Regards,
Luiz Marangoni
lc_marangoni@bol.com.br



>Hi All,
>I am trying to deposit 20 microns of Aluminum in Evaporation or in
>Sputtering.
>However, the film is very stress (more stress in sputtering).
>Do you know a way to reduce the stress for such films?
>
>
>My Best Regards,
>Lior Grossman; Sales Manager
>B.G. Technical Support Ltd (www.bg-tech.co.il)
>_______________________________________________
>mems-talk@memsnet.org mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.mems-exchange.org/
>
>
>
>---
>Incoming mail is certified Virus Free.
>Checked by AVG anti-virus system (http://www.grisoft.com).
>Version: 6.0.307 / Virus Database: 168 - Release Date: 11/12/01

reply