[IMAGE] Hi I want to make circular cone shapes(with metal) on the metal layer using lift-off process I had asked here before. (Thanks for many kind andswers! But my explanation was not enough.) A diameter of the base plane must be about 50um and the height of the cone must be 75~80um. The hard points of this method are, 1. to make this shape using lift-off process. Is it possible to make a suitable structure using negative photoresist? (75~80um) 2. to make all of the cones' height regular. I have no experience in lift-off process. Is it possible to make many cones uniform? 3. to make the structure. How can I make the cones with Ni(maybe) or its alloy? (ex. sputtering...?) If you have an ideas, let me know, please. Thanks.