durusmail: mems-talk: AZ5214
AZ5214
2002-01-09
2002-01-10
2002-01-14
2002-01-10
AZ5214
Mac McReynolds
2002-01-10
Contact Clariant Corporation, Business Unit Electronic Materials,
Somerville, NJ 800-515-4164

Mac McReynolds
R&D Manager
Caliper Technologies Corp.
605 Fairchild Drive
Mountain View, CA 94043-2234
Tel:  650-623-0710
Fax:  650-623-0521

> ----------
> From:         shaoning
> Reply To:     mems-talk@memsnet.org
> Sent:         Wednesday, January 9, 2002 12:37 PM
> To:   mems-talk@memsnet.org
> Subject:      [mems-talk] AZ5214
>
> Hello, everybody,
>
> Does anyone know the contact info of manufacturer or vendor of AZ5214
> photoresist? It is said it can be reversed from positive to negative
> polarity
> by different baking. Thank you very much for every information.
>
> Shaoning
> _______________________________________________
> mems-talk@memsnet.org mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/