Hi folks !

I am looking for some advices to get a very uniform surface of nickel
electroplated layers (especially on silicon). Through my bibliography research,
it seems that the trick is mainly to get an uniform current density across the
coated surface (parallel current lines). The problem is the resist pattern wich
does'nt allow to obtain that kind of strictly vertical current lines. Does
anyone has an ingenious idea or a good web address to help me overcoming such a
problem, please ?