How deep? Vic ----- Original Message ----- From: Dlee LiTo: Sent: Tuesday, February 19, 2002 5:26 PM Subject: [mems-talk] Drill diameter 100um in thick glass wafer > I need to drill diameter 100um in thick glass wafer(thickness is from 1mm to > 3mm). would you like to help me to figure out some way or which company can > do that? > > thanks for your any information > > Dlee > Research Asistant > Mechanical Engineering Department > University of Texas At Austin, TX > > _________________________________________________________________ > MSN Photos is the easiest way to share and print your photos: > http://photos.msn.com/support/worldwide.aspx > _______________________________________________ > mems-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.mems-exchange.org/