Many plumbers who specialize in gas lines have orbital welders. These welders
are fairly complex to use and also require gas purging of both the weld and
the gas line to ensure a proper weld. In addition Unit Instruments makes an
orbital welder for sale.

Sincerely,
Walter Stonas
Process Development Engineer

-----Original Message-----
From: Michael D Martin [mailto:michael.martin@louisville.edu]
Sent: Monday, February 25, 2002 1:17 PM
To: mems-talk@memsnet.org
Subject: [mems-talk] Orbit welding


Hi all,
   Does anyone out there have a used orbit welder they would be
interested in selling? Can you suggest a vendor, other than Bidservice?

Thanks,
    Michael Martin
    U of Louisville
_______________________________________________
mems-talk@memsnet.org mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply