Gaoshan-

We routinely use OptiClear solutions 101 and 102 on post wafer dicing clean.
They are probably citrus based, judging by their characteristic odor.

See the manufacturer's site, National Diagnostics, clicking on the tab
"ElectroOptical Solvents"
http://www.nationaldiagnostics.com/ 
Regards,


Michael Alderete
Lead Mechanical Packaging Engineer
DRS Sensors & Targeting Systems, Inc.
3400 E. Miraloma Ave Bldg 241-2
Anaheim CA 92806

michael.alderete@boeing.com
TEL (714) 762-2814
FAX (714) 762-6105

You wrote...
Message: 17
From:   "Gaoshan Jing"  >
To:      >
Date:   Mon, 25 Feb 2002 20:48:54 -0500
Subject:        [mems-talk] about Opticlear
        Reply-To: mems-talk@memsnet.org 

Hi:
Does anybody know what is the ingredient of Opticlear which can remove wax?
Or just give me a website about detail information about it.  Thanks a lot.
Gaoshan Jing