Hi, Effective solvents for removing Apiezon. Black Wax are Xylene,Toluene (not necessarily hot) and Chlorinated hydrocarbons such as Methylene Chloride and Trichloroethylene. Aliphatic hydrocarbons such as Hexane can also be used but they are not as effective. The Wax is INSOLUBLE in Ketones such as Acetone and in Alcohols such as Ethanol and Iso Propanol. Dave Summers Technical Service Manager Apiezon Products Ltd. ********************************* ----- Original Message ----- From: Maurice NorcottTo: Sent: 26 February 2002 17:26 Subject: RE: [mems-talk] black wax > Try Ted Pella or SPI, both electron microscopy supply houses. I think > VWR may carry Apiezon black wax also. Acetone or hot toluene will remove > the wax, followed with isopropyl rinse. > > -----Original Message----- > From: ABHIJAT GOYAL [mailto:abhijatgoyal@psu.edu] > Sent: Monday, February 25, 2002 7:13 PM > To: mems-talk@memsnet.org > Subject: [mems-talk] black wax > > > Hi, > > can you please suggest me some vendors for Black Wax as a mask for KOH > etch. > Can you please tell me the vendors that are based in US only, since it will > be > difficult for me to procure my order if they are outside the US. > > Also can you please suggest me something by which I can remove black wax > after I have etched. > > Thanks in advance, > > Abhijat Goyal > > > Abhijat Goyal > EE MEMS group, > MS candidate, > Dept. Of Electrical Engineering, > State College, PA > > Ph: (R)814-2350917 > (O)814-8653664 > _______________________________________________ > mems-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.mems-exchange.org/ > _______________________________________________ > mems-talk@memsnet.org mailing list: to unsubscribe or change your list > options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk > Hosted by the MEMS Exchange, providers of MEMS processing services. > Visit us at http://www.mems-exchange.org/ > > ________________________________________________________________________ > This e-mail has been scanned for all viruses by Star Internet. The > service is powered by MessageLabs. For more information on a proactive > anti-virus service working around the clock, around the globe, visit: > http://www.star.net.uk > ________________________________________________________________________ > ________________________________________________________________________ This e-mail has been scanned for all viruses by Star Internet. The service is powered by MessageLabs. For more information on a proactive anti-virus service working around the clock, around the globe, visit: http://www.star.net.uk ________________________________________________________________________