durusmail: mems-talk: Anodic bonding glass-titanium
Anodic bonding glass-titanium
2002-03-01
2002-03-01
2002-03-01
2002-03-05
Anodic bonding glass-titanium
Roger Shile
2002-03-01
I tried unsucessfully to bond Pyrex to a chrome film in air.  However someone
on this forum indicated they were able to do this in a nitrogen ambient.

I understand that many metals can be andoically bonded to Pyrex.  The trick
may be to prevent excessive oxidation of the metal during bonding.

Roger Shile



>>> lteyssed@altern.org 03/01/02 02:06AM >>>
I tried to make anodic bonding between glass and titanium but it was
unsuccessful.  Have you any idea about why it didn't succeed ?

Thank you in advance.